Injection Molding Wall Thickness: Practical Rules That Prevent Sink and Warp

By Mohamed Emara, Mechanical Design Engineer · 2026-11-23

Most molding defects we see in client parts trace back to one thing: walls that change thickness without a reason. Plastic shrinks as it cools, and thick areas cool last, pulling the surface in (sink) or bending the part (warp).

Rule 1: keep walls uniform

Pick a nominal wall and hold it across the part. Where thickness must change, transition gradually over a length of about three times the difference instead of a step.

Rule 2: use typical ranges for your material

MaterialTypical wall (mm)
ABS1.2 to 3.5
PC1.0 to 4.0
PP0.8 to 3.0
PA (Nylon)0.8 to 3.0

Treat these as starting points and confirm with your molder for the specific grade and part size.

Rule 3: ribs instead of thickness

If a wall needs to be stiffer, add ribs rather than thickening it. Keep rib thickness around 50 to 60 percent of the wall it sits on, height under three times the wall, and add draft.

Rule 4: core out bosses and thick features

Screw bosses should be hollow with walls close to the nominal thickness and connected to side walls with ribs, not solid blocks of plastic.

Rule 5: radius the corners

An inside radius of about half the wall thickness (and an outside radius of inside plus one wall) keeps thickness constant around corners and reduces stress.

Want a second pair of eyes before tooling? Our free DFM review checks walls, draft and undercuts on your STEP file.